The temperature required for full annealing in hyper-eutectoid steel is
50°C above upper critical temperature
50°C below upper critical temperature
50°C above lower critical temperature
50°C below lower critical temperature
Answer: Option
Explanation:
No answer description is available. Let's discuss.
Discussion:
12 comments Page 2 of 2.

Sagar said:   9 years ago
I think option c is right.

Jai maurya said:   1 decade ago
50 Degree above lower critical temp for hyper eutectoid.