The temperature required for full annealing in hyper-eutectoid steel is
Discussion:
12 comments Page 1 of 2.
Vanraj Gajarotar said:
6 years ago
C is a right answer because 50° above upper critical temperature is for hypo eutectoid steel and 50° above lower critical temperature is for hypereutectoid steel.
Jai maurya said:
1 decade ago
50 Degree above lower critical temp for hyper eutectoid.
Deepak said:
7 years ago
The answer stated is for hypo-eutectoid steels.
P Das said:
8 years ago
50°C above lower critical temperature.
Shivaprasad said:
7 years ago
The Correct answer is A. Ref: R S Khurmi.
Guru said:
9 years ago
Yes, the answer is C, as per RS Khurmi.
ATC said:
8 years ago
C is correct. For hypo it is correct.
Dinesh said:
8 years ago
I think C is the correct answer.
Sagar said:
9 years ago
I think option c is right.
Neeraj said:
9 years ago
C is correct. I too agree.