The temperature required for full annealing in hyper-eutectoid steel is
50°C above upper critical temperature
50°C below upper critical temperature
50°C above lower critical temperature
50°C below lower critical temperature
Answer: Option
Explanation:
No answer description is available. Let's discuss.
Discussion:
12 comments Page 1 of 2.

Jai maurya said:   1 decade ago
50 Degree above lower critical temp for hyper eutectoid.

Sagar said:   9 years ago
I think option c is right.

Sandip said:   9 years ago
Ans is C, as per S.CHAND.

Guru said:   9 years ago
Yes, the answer is C, as per RS Khurmi.

Neeraj said:   9 years ago
C is correct. I too agree.

Dinesh said:   8 years ago
I think C is the correct answer.

P Das said:   8 years ago
50°C above lower critical temperature.

Anil reddy said:   8 years ago
C is correct answer.

ATC said:   8 years ago
C is correct. For hypo it is correct.

Deepak said:   7 years ago
The answer stated is for hypo-eutectoid steels.