Civil Engineering - Building Materials - Discussion

Discussion Forum : Building Materials - Section 3 (Q.No. 2)
2.
Initial setting of cement is caused due to
Tri-calcium silicate
Di-calcium silicate
Tri-calcium aluminate
Tetra calcium alumino ferrite.
Answer: Option
Explanation:
No answer description is available. Let's discuss.
Discussion:
27 comments Page 3 of 3.

Sunil kumawat said:   7 years ago
C3A is responsible for both flash and initial setting time.

Priyanka said:   4 years ago
Early strength - C3S.
Early setting - C3A.
(1)

Chandrima said:   8 years ago
I think it is Tri calcium silicate.

Him said:   4 years ago
I'm agree with you, Thanks @Joey.

Muttu said:   6 years ago
Option A is the correct answer.

Black lover said:   4 years ago
I think option A is correct.
(1)

Ramavtar said:   8 years ago
C3S is correct.