A casting defect which occurs near the ingates as rough lumps on the surface of a casting is known as
Discussion:
3 comments Page 1 of 1.
Nvk said:
1 year ago
The correct answer is scab.
A scab is a type of casting defect that occurs near the ingates (where the molten metal enters the mould) as rough lumps on the surface of a casting. Scabs are caused by:
- Metal penetrating the sand mould and solidifying under the surface.
- Sand grains or mould material becoming embedded in the metal surface.
Scabs can be caused by:
- Poor mould design or construction
- Insufficient sand compaction
- Incorrect pouring techniques
Here's why the other options are incorrect:
- Shift: A shift is a casting defect that occurs when the mould is not properly aligned, resulting in a mismatch between the cope and drag.
- Sand wash: Sand wash is a casting defect that occurs when the molten metal erodes the sand mould, creating a rough surface.
- Swell: Swell is a casting defect that occurs when the molten metal expands and solidifies, creating a bulge or protrusion on the surface of the casting.
Note: Casting defects can be caused by a variety of factors, including mould design, material selection, and pouring techniques. Identifying and correcting the root cause of a defect is crucial to producing high-quality castings.
A scab is a type of casting defect that occurs near the ingates (where the molten metal enters the mould) as rough lumps on the surface of a casting. Scabs are caused by:
- Metal penetrating the sand mould and solidifying under the surface.
- Sand grains or mould material becoming embedded in the metal surface.
Scabs can be caused by:
- Poor mould design or construction
- Insufficient sand compaction
- Incorrect pouring techniques
Here's why the other options are incorrect:
- Shift: A shift is a casting defect that occurs when the mould is not properly aligned, resulting in a mismatch between the cope and drag.
- Sand wash: Sand wash is a casting defect that occurs when the molten metal erodes the sand mould, creating a rough surface.
- Swell: Swell is a casting defect that occurs when the molten metal expands and solidifies, creating a bulge or protrusion on the surface of the casting.
Note: Casting defects can be caused by a variety of factors, including mould design, material selection, and pouring techniques. Identifying and correcting the root cause of a defect is crucial to producing high-quality castings.
Tahir said:
9 years ago
Scabs are a thin layer of metal that sits proud of the casting.
A swell occurs when the mold wall gives way across a whole face and is caused by an improperly rammed mold.
A swell occurs when the mold wall gives way across a whole face and is caused by an improperly rammed mold.
Shiva said:
7 years ago
It's scab.