The cracks caused by shrinkage of the exterior surface of the wood exposed to atmosphere, are called:
radial shakes
heart shakes
wind cracks
twisted fibres.
Answer: Option
Explanation:
No answer description is available. Let's discuss.
Discussion:
11 comments Page 2 of 2.

Surendra s Dangi said:   8 years ago
Heart shake is a crack in the heartwood, near the centre of the tree. It is caused by poor seasoning, or by using trees felled past maturity.

A crack or cracks propagating from near the edge of the log towards the centre, usually along the line of the medullary rays.

Answer C.